An article Modified silica-based isoprene rubber composite by a multi -functional silane: Preparation and its mechanical and dynamic mechanical properties WOS:000581970300084 published article about FILLER-ELASTOMER INTERACTIONS; EPOXIDIZED NATURAL-RUBBER; COUPLING AGENTS; SURFACE MODIFICATION; NANOCOMPOSITES; NANOPARTICLES; PARTICLES; TIME in [Wang, Xuefei; Li, Huaming; Yang, Jun] Xiangtan Univ, Coll Chem, Xiangtan 411105, Hunan, Peoples R China; [Wang, Xuefei; Wu, Lingling; Yu, Haiwen; Xiao, Tongliang; Yang, Jun] Zhuzhou Times New Mat Technol Co Ltd, Zhuzhou 412007, Hunan, Peoples R China in 2020.0, Cited 42.0. HPLC of Formula: C4H14Cl2N2S2. The Name is 2,2′-Disulfanediyldiethanamine dihydrochloride. Through research, I have a further understanding and discovery of 56-17-7
Modified silica-based isoprene rubber (IR) composite has been designed and prepared by using a multi-functional silane, 2-aminoethyl 2-(3-triethoxysilylpropyl)aminoethyl disulfide (ATD), as coupling agent. Such modification significantly improved the dispersity of silica in the corresponding composites, as verified by SEM observation. And the hardness, tensile strength, stress at definite elongation, tear strength and temperature rise as well as the value of dynamic loss coefficient ranging from 0 degrees C to 80 degrees C of silica/IR vulcanized composites, are significantly improved, especially with low ATD dosage (2-4 phr). This modification of silica-based IR composite by employing ATD as coupling agent provides a facile and effective method to prepare silica-based rubber composites with improved mechanical properties and low hysteresis.
HPLC of Formula: C4H14Cl2N2S2. Bye, fridends, I hope you can learn more about C4H14Cl2N2S2, If you have any questions, you can browse other blog as well. See you lster.
Reference:
Thiazine – an overview | ScienceDirect Topics,
,Thiazine | C4H5NS – PubChem